Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 36.2 GPa | 5250 ksi | ASTM D790 |
Techmer ES Elastoblend® PA6/6 GF13 IM HS BK 13% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 13% Filler by WeightAdditive: Heat Stabilizer, Impact Modifier and LubricantFeatures: Heat Stabilized, Impac.. |
|||
Flexural Modulus | 36.2 GPa | 5250 ksi | ASTM D790 |
Techmer ES Elastoblend® PA6/6 GF13 IM HS L 13% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 13% Filler by WeightAdditive: Heat Stabilizer and Impact ModifierFeatures: Heat Stabilized and Impact Modifi.. |