Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 24.61 GPa | 3569 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP STAT-KON RE007 PA 66 LNP* STAT-KON* RE007 is a compound based on PA66 resin containing 35% Carbon Fiber. Added features include: Electrically Conductive. |