Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 2.322 GPa | 336.8 ksi | chs 0.05 in/min; tangent; ASTM D790 |
Diamond Polymers NPP 808 C5 TDS Polycarbonate Alloy Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |