Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 21.65 GPa | 3140 ksi | ISO 178 |
SABIC Innovative Plastics LNP Thermocomp LC006E PEEK LNP THERMOCOMP* LC006E is a compound based on Polyetheretherketone resin containing Carbon Fiber. Added features of this material include: Easy Molding.This data was supplied by SABIC-IP for the Am.. |