Mechanical Properties Metric English Comments
Flexural Modulus 21.379 GPa
3100.8 ksi
ASTM D-790
PlastiComp Complet® LGF60 - PA6 Nylon 6, 60% Long Glass Fiber Reinforced
Complet® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Nylon 6 with 60% long glass reinforcementInformation provided by PlastiComp, Inc.