POLYMER SEARCH
Polymer Property : Flexural Modulus = 310.1 ksi
Polymer Property :
Flexural Modulus =
310.1 ksi
Product List
Mechanical Properties
Tips:
30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties
Metric
English
Comments
Flexural Modulus
2.138
GPa
310.1
ksi
tangent; ASTM D790
Entec Hypro™ PPC-GF10 Natural Impact Polypropylene, 10% Glass Reinforced
Information provided by Entec