Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 2.137 GPa | 310.0 ksi | ASTM D790 |
RedEye On Demand Polycarbonate High Impact Strength & Temperature Resistant for Rapid Prototyping Polycarbonate (PC) is an actual industrial-grade thermoplastic that is impact-resistant and structurally strong. PC parts are built with a layered manufacturing process utilizing Fused Deposition Mo.. |
|||
Flexural Modulus | 2.137 GPa | 310.0 ksi | ASTM D790 |
RedEye On Demand VeroBlack PolyJet™ FC870 for Rapid Prototyping Vero PolyJet Resin (VeroBlue™ FC840 & VeroBlack™ FC870) is a photopolymer resin designed for precise jetting in super fine layers by PolyJet™ Technology, often used in rapid prototyping. Our Vero.. |
|||
Flexural Modulus | 2.137 GPa | 310.0 ksi | ASTM D790 |
RedEye On Demand VeroWhite PolyJet Resin White for Rapid Prototyping Vero PolyJet Resin (VeroBlue™ FC840 & VeroBlack™ FC870) is a photopolymer resin designed for precise jetting in super fine layers by PolyJet™ Technology, often used in rapid prototyping. Our Vero.. |
|||
Flexural Modulus | 2.137 GPa | 310.0 ksi | ASTM D790 |
Ineos Nova 5730 High flow, High impact
(discontinued **) High flow, High impact, USP Class VIApplications: Toys, Medical, HousewaresProperties were determined on injection molded specimens at 23°C and 50% R.H. unless otherwise specified.Information provi.. |
|||
Flexural Modulus | 2.137 GPa | 310.0 ksi | ASTM D790 |
Eastman Tenite 105E3V36327 Acetate Clear, Trsp Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel. The mechanical properties if Tenite cellulosi.. |
|||
Flexural Modulus | 2.137 GPa | 310.0 ksi | XY direction; ASTM D790 |
ALM PA 850-Nat Nylon 11 SLS Prototyping Polymer Unfilled PA 11 formulated for easy processing. Can be run as a drop-in replacement for other commercially available PA 11 laser sintering powders. Parts produced from PA 850 exhibit outstanding mech.. |
|||
Flexural Modulus | 2.137 GPa | 310.0 ksi | ASTM D790 |
Ineos Nova 5711 High Impact Polystyrene
(discontinued **) High flow, High impact, USP Class VIApplications: Thin wall, Medical, Housewares, ToysProperties were determined on injection molded specimens at 23°C and 50% R.H. unless otherwise specified.Inform.. |