Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 0.216 GPa @Thickness 6.40 mm |
31.3 ksi @Thickness 0.252 in |
15mm/min; ASTM D790 |
LG Chemical KEYFLEX BT 1163D Ester Type TPE Description: Injection Molding, TPC-ET, General Purpose, High ModulusApplication: Cable & Wire Jackets, Hose & Tubing, SheetCAS: 37282-12-5Information provided by LG Chemical |
|||
Flexural Modulus | 0.216 GPa @Temperature -20.0 °C |
31.3 ksi @Temperature -4.00 °F |
ASTM D790 |
DuPont Elvax® 460 Ethylene-Vinyl Acetate Copolymer Resin Elvax resins offer a unique combination of processing and performance characteristics. They provide outstanding toughness and resilience and maintain flexibility over a broad temperature range with.. |