Mechanical Properties Metric English Comments
Flexural Modulus 2.135 GPa
309.7 ksi
ASTM D790
A. Schulman PP 3471-01 Polypropylene High Flow Homopolymer Polypropylene
DescriptionPolypropylene PP 3471-01 is an ultra high flow homopolymer polypropylene designed for high speed, thin wall injection molding.Information provided by A. Schulman.
Flexural Modulus 2.135 GPa
309.7 ksi
ASTM D790
A. Schulman PP 3471-01 Polypropylene High Flow Homopolymer Polypropylene
DescriptionPolypropylene PP 3471-01 is an ultra high flow homopolymer polypropylene designed for high speed, thin wall injection molding.Information provided by A. Schulman.
Flexural Modulus 2.135 GPa
309.7 ksi
ASTM D790
A. Schulman PP 3471-01 Polypropylene High Flow Homopolymer Polypropylene
DescriptionPolypropylene PP 3471-01 is an ultra high flow homopolymer polypropylene designed for high speed, thin wall injection molding.Information provided by A. Schulman.
Flexural Modulus 2.135 GPa
309.7 ksi
ASTM D790
A. Schulman PP 3471-01 Polypropylene High Flow Homopolymer Polypropylene
DescriptionPolypropylene PP 3471-01 is an ultra high flow homopolymer polypropylene designed for high speed, thin wall injection molding.Information provided by A. Schulman.
Flexural Modulus 2.135 GPa
309.7 ksi
ASTM D790
A. Schulman PP 3471-01 Polypropylene High Flow Homopolymer Polypropylene
DescriptionPolypropylene PP 3471-01 is an ultra high flow homopolymer polypropylene designed for high speed, thin wall injection molding.Information provided by A. Schulman.
Flexural Modulus 2.135 GPa
309.7 ksi
ASTM D790
A. Schulman PP 3471-01 Polypropylene High Flow Homopolymer Polypropylene
DescriptionPolypropylene PP 3471-01 is an ultra high flow homopolymer polypropylene designed for high speed, thin wall injection molding.Information provided by A. Schulman.
Flexural Modulus 2.135 - 2.265 GPa
309.7 - 328.5 ksi
ASTM D790M
DSM Somos® ProtoCast™ AF 19122 Antimony-free Liquid Photopolymer
Product DescriptionDSM Somos® ProtoCast™ AF 19122 is an antimony-free liquid photopolymer specifically formulated for producing investment casting patterns.ApplicationsIdeal for use in foundry app..