Polymer Property : Flexural Modulus = 308.4 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 2.126 - 2.314 GPa
308.4 - 335.6 ksi
ASTM D790M
DSM Somos® ProtoGen™ 18920 Liquid Photopolymer, UV Postcure
Product DescriptionDSM Somos® ProtoGen 18920 is a liquid photopolymer that produces accurate, ABS-like parts ideal for general purpose applications. ProtoGen resins are the first SL resins to demo..