Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 20.69 GPa | 3001 ksi | ASTM D-790 |
PlastiComp Velocity® LCF40-PA66 High Flow Nylon 66, 40% Long Carbon Fiber This compound complies with European Union Directive 2002/95/EC Restriction of Hazardous Substances (RoHS).Information provided by PlastiComp, Inc. |