Mechanical Properties Metric English Comments
Flexural Modulus 3.98 GPa
577 ksi
ASTM D790
SABIC Innovative Plastics LNP THERMOCOMP AX90213 ABS
LNP* THERMOCOMP* AX90213 is a compound based on ABS resin containing Glass Fiber.
Flexural Modulus 3.98 GPa
577 ksi
ASTM D790
SABIC Innovative Plastics LNP THERMOCOMP AX90213 ABS (Asia Pacific)
LNP* Thermocomp* AX90213 is a compound based on Acrylonitrile Butadiene Styrene resin containing Glass Fiber.
Flexural Modulus 3.98 GPa
577 ksi
1.3 mm/min, 50 mm span; ASTM D 790
SABIC Innovative Plastics LNP Thermocomp WB006 PBT
LNP* Thermocomp* WB006 is a compound based on Polybutylene Terephalate resin containing Glass Bead.This data was supplied by SABIC-IP for the Americas region.