Polymer Property : Flexural Modulus = 3.94 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 3.94 GPa
571 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics Valox® 4012G PBT
VALOX 4012G is a 10% glass fiber reinforced PBT injection molding resin with excellent mechanical properties. Applications: connectors. This grade is a 4012 with improved cycle time and ductility.
Flexural Modulus 3.94 GPa
571 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics LNP THERMOCOMP ZX06323 PPE+HIPS (Asia Pacific)
This material is mineral filled PPO grade with high dielectric constant and low loss tangent