Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 3.825 GPa | 554.8 ksi | ASTM D790 |
Kolon SPESIN® KP513MT25 G/F Reinforced PBT Alloy Resin High flow, dimensionally stableApplications: Head lamp bezelsInformation provided by API-Kolon. |
|||
Flexural Modulus | 3.825 GPa | 554.8 ksi | ASTM D790 |
Daelim H&L Plavis-G15 ISO 15% Graphite Filled Aromatic Polyimide Bearing Isostatically Molded. Plavis-G-15: Graphite 15 wt% filled, Self lubricating grade for wear and friction applications.General Plavis information for all grades:PLAVIS polyimide has nitrogen bonded .. |