Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 0.0250 GPa | 3.63 ksi | ISO 178 |
Huntsman AVALON® 80 ABU Thermoplastic Polyurethane Introduction: AVALON 80 ABU is a high performance UV-stabilized polyester based thermoplastic polyurethane for injection molding. AVALON 80 ABU is part of the AVALON Perform Range and offers a premi.. |
|||
Flexural Modulus | 0.0250 GPa | 3.63 ksi | ISO 178 |
Huntsman AVALON® 80 AB Thermoplastic Polyurethane Introduction: AVALON 75 AB is a high performance polyester based thermoplastic polyurethane for injection molding. AVALON 75 AB is part of the AVALON Performance Range and offers a premium soling ma.. |
|||
Flexural Modulus | 0.0250 GPa | 3.63 ksi | ASTM D790 |
Arkema Group Pebax® 3533 Polyether Block Amide (PEBA) Information provided by Arkema Group |
|||
Flexural Modulus | 0.0250 GPa @Thickness 2.00 mm |
3.63 ksi @Thickness 0.0787 in |
molded plaque, cured 20 hr at 100°C; ASTM D790 |
BASF Elastollan® 1175A10W Wire & Cable Grade Polyurethane Elastomer As with all TPU products this grade must be dried prior to processing.Information provided by BASF Corporation. |
|||
Flexural Modulus | 0.0250 GPa | 3.63 ksi | ISO 178 |
DuPont Performance Polymers Hytrel® G3548 NC010 Polyester Elastomer TPC-ET
(Unverified Data**) 35 Shore D Standard Performance Polyester Elastomer with Non-discoloring StabilizerInformation provided by DuPont Performance Polymers |