Polymer Property : Flexural Modulus = 3.60 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 0.0248 GPa
3.60 ksi
1% Secant; ASTM D790
M. Holland Company LD505 LDPE  (discontinued **)
Additives: 0.050 % Slip Features: High Flow, Medium GlossUses: Household Goods, ToysProcessing Method: Injection MoldingInformation provided by M. Holland.
Flexural Modulus 0.0248 GPa
3.60 ksi
1% secant; ASTM D790
ExxonMobil OPTEMA™ TC 220 Molding Ethylene Methyl Acrylate
OPTEMA TC 220 is an ethylene methyl acrylate copolymer, which can be used in specialty bonding applications and as a toughener for engineering polymers. It can been processed at temperatures as low ..
Flexural Modulus 0.0248 - 0.862 GPa
3.60 - 125 ksi
Average value: 0.217 GPa Grade Count:94
Overview of materials for Low Density Polyethylene (LDPE), Molded
This property data is a summary of similar materials in the MatWeb database for the category "Low Density Polyethylene (LDPE), Molded". Each property range of values reported is minimum and maximum ..