Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 3.588 GPa | 520.4 ksi | ASTM D790 |
LG Chemical IH830A PMMA, General Purpose Grade for Injection Molding Highest of all grades in heat resistanceMechanical strength and surface hardnessParticularly recommended for tail lamp, reflectors, and general lighting fixturesFeatures: Excellent transparency and .. |