Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 0.0241 GPa | 3.50 ksi | ASTM D790 |
Techmer ES HiFill® ABS 0350 Availability: North AmericaFeatures: High DensityForms: PelletsProcessing Method: Extrusion MoldingInformation provided by TP Composites, Inc. |
|||
Flexural Modulus | 0.0241 - 6.89 GPa | 3.50 - 1000 ksi | Average value: 2.34 GPa Grade Count:305 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Molded This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Molded". Each property range of values reported is minimum and ma.. |