Mechanical Properties Metric English Comments
Flexural Modulus 3.378 GPa
489.9 ksi
ASTM D790
Ineos Nova 3700 General Purpose Crystal Polystyrene  (discontinued **)
Good balance of flow and strength, Good crack resistanceApplications: Single service wares, Blending resinExposure to gamma radiation in the 2.02-6.06 megarad range has no significant effect on the ..