Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 3.37 GPa | 489 ksi | 2.6 mm/min, 100 mm span; ASTM D790 |
SABIC Innovative Plastics ULTEM 1285 PEI Transparent Polyetherimide blend. ECO Conforming. US FDA and EU Food Contact Compliant in recognized colors. |
|||
Flexural Modulus | 3.37 GPa | 489 ksi | 2.6 mm/min, 100 mm span; ASTM D790 |
SABIC Innovative Plastics ULTEM 1285 PEI (Asia Pacific) Transparent Polyetherimide blend. ECO Conforming. US FDA and EU Food Contact compliant in recognized colors. |
|||
Flexural Modulus | 3.37 GPa | 489 ksi | ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP DFZ22P PC (Asia Pacific) LNP* THERMOCOMP* DFZ22P is a compound based on Polycarbonate resin containing Glass Fiber, Milled Glass. Added features of this material include: Exceptional Processing. |
|||
Flexural Modulus | 3.37 GPa | 489 ksi | ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP DFZ22P PC LNP THERMOCOMP* DFZ22P is a compound based on Polycarbonate resin containing 10% Glass Fiber, 10% Milled Glass. Added features of this material include: Exceptional Processing. |
|||
Flexural Modulus | 3.37 GPa | 489 ksi | ASTM D790 |
Tipco Tipcolene® FPT 20 FR VO LTHA - UL94-V0 Flame Retardant, 20% Talc Polypropylene Homopolymer, Long Term Heat Stability 20% Talc Reinforced PP Homopolymer with Long Term Heat StabilityApplications: Electrical & AppliancesProcessing: Injection MoldingInformation provided by the Manufacturer, Tipco Industries Ltd.,
Ind.. |