Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 2.28 - 3.03 GPa | 331 - 439 ksi | Average value: 2.81 GPa Grade Count:12 |
Overview of materials for PVC, Transparent This property data is a summary of similar materials in the MatWeb database for the category "PVC, Transparent". Each property range of values reported is minimum and maximum values of appropriate M.. |