Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 1.9871 GPa @Thickness 3.20 mm |
288.21 ksi @Thickness 0.126 in |
1.3mm/min; ASTM D790 |
LG Chemical LUCEL FW715CS Modified POM, Friction Resistance, Abrasion Resistance Feature: Injection Molding, Modified POM, Friction Resistance, Abrasion ResistanceApplication: Gears, Printer Roller Pumps, Gear Worm WheelsCAS No. 66455-31-0 and 471-34-1Information provided by LG .. |