Polymer Property : Flexural Modulus = 2870 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 19.8 GPa

@Temperature 150 °C
2870 ksi

@Temperature 302 °F
ASTM D790
Mitsui AURUM® JCN6230 Thermoplastic Polyimide Resin, Crystalline  (discontinued **)
AURUM® is an easy melt, processable and recyclable thermoplastic polyimide resin that provides continuous service temperatures to 465° F in its amorphous state and up to 550° F when annealed to i..
Flexural Modulus 19.8 GPa
2870 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics LNP LUBRICOMP LCL36E PEEK (Europe-Africa-Middle East)
LNP* LUBRICOMP* LCL36E is a compound based on Polyetheretherketone resin containing Carbon Fiber , PTFE. Added features include : Electrically Conductive, Internally Lubricated, Easy Molding.
Flexural Modulus 19.8 GPa
2870 ksi
2 [mm/min]; ISO 178
Akro-Plastic Akromid® A3 GF 60 (2424) PA 6.6 Dry, 60% Glass Filled
AKROMID® A (Polyamide 6.6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperat..