Polymer Property : Flexural Modulus = 2816 ksi
Polymer Property :
Flexural Modulus =
2816 ksi
Product List
Mechanical Properties
Tips:
30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties
Metric
English
Comments
Flexural Modulus
19.42
GPa
2816
ksi
ASTM D790
PolyOne Therma-Tech™ NJC-6500 Nylon 12 (discontinued **)
PolyOne First ChoiceInformation provided by PolyOne Corporation.