Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 1.932 GPa | 280.2 ksi | tangent; chs 0.05 in/min; ASTM D790 |
Diamond Polymers DIAMALOY 223U UV Stabilized, PC/PET Alloy Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |