Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 28.4 GPa | 4120 ksi | ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP RC008 PA 66 LNP THERMOCOMP* RC008 is a compound based on Nylon 66 resin containing 40% Carbon Fiber. Added features of this material include: Electrically Conductive. |