Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 28.3 GPa @Temperature 23.9 °C |
4100 ksi @Temperature 75.0 °F |
Dry; ASTM D790 |
Park Electrochemical Nelcote® E-722 Epoxy Prepreg, 285 Aramid Reinforced Nelcote® E-722 is a modified 350°F cure epoxy system with excellent processing characteristics for vacuum bag, press, and autoclave molding.Key Features and Benefits:Epoxy resin system optimized f.. |
|||
Flexural Modulus | 28.3 GPa | 4100 ksi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics LNP Thermocomp OC008A PPS - Branched LNP* Thermocomp* OC008A is a compound based on Branched Polyphenylene Sulfide containing Carbon Fiber.This data was supplied by SABIC-IP for the Americas region. |
|||
Flexural Modulus | 28.3 GPa @Temperature 23.0 °C |
4100 ksi @Temperature 73.4 °F |
|
Hexcel® HexPly® 954-2A Curing Cyanate Resin, S-2 Glass Fiber Reinforced 8 Harness Satin Fabric Information provided by HexCel |