Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 19.292 GPa @Thickness 3.17 mm |
2798.1 ksi @Thickness 0.125 in |
chs 0.05 in/min; ASTM D790 |
Diamond Polymers DIAMALOY 1001 CF40 40% Carbon Fiber Filled ABS Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |