Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Flexural Modulus = 278.8 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 1.922 GPa

@Thickness 3.17 mm
278.8 ksi

@Thickness 0.125 in
chs 0.05 in/min; 2 in span; ASTM D790
Diamond Polymers DIAMALOY GLY 7010 Sheet Extrusion Grade
Diamaloy GLY 7010 resin is a high-gloss, high impact grade of ASA (acrylonitrile-styrene-acrylate) with good resistance to weather aging. It has good melt strength for extrusion and thermoforming, a..