Flexural Modulus 1.876 GPa
272.1 ksi
ASTM D790
Lucent Polymers PC/PBT-1830 Polycarbonate+PBT, Superior Cold Temp Impact, Injection Grade
Add "R" for Added ReleaseAdd "U" for UV StabilizerInformation provided by Lucent Polymers, Inc.