Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 1.87 GPa | 272 ksi | 2.8 mm/min; ASTM D790 |
Samsung Cheil Industries Starex® GC-0710 ABS/PET, Unreinforced Recycled Eco-friendly Post-Consumer recycled PET.Information provided by Samsung Cheil Industries. |
|||
Flexural Modulus | 1.87 GPa | 272 ksi | 2.8 mm/min; ASTM D790 |
Samsung Cheil Industries Starex® GC-0710 ABS/PET, Unreinforced Recycled Eco-friendly Post-Consumer recycled PET.Information provided by Samsung Cheil Industries. |