Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 18.61 GPa | 2699 ksi | ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP QC006 PA 6/10 (Asia Pacific) LNP* THERMOCOMP* QC006 is a compound based on Nylon 6/10 resin containing Carbon Fiber. Added features of this material include: Electrically Conductive. |