Mechanical Properties Metric English Comments
Flexural Modulus 18.56 GPa
2692 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics LNP THERMOCOMP EC005R PEI
LNP* THERMOCOMP* EC005R is a compound based on Polyetherimide resin containing 25% Carbon Fiber. Added features include: Mold Release, Electrically Conductive.