Mechanical Properties Metric English Comments
Flexural Modulus 1.860 GPa
269.8 ksi
ASTM D790
KKPC Kuhmo MIB 237 Blow Molding HIPS
Key features: Good-profiling, Thin-layer Molding. Common Uses: It is used exclusively as a container for fermented milk beverages.HIPS is a functional resin made by copolymerization of styrene monom..