Mechanical Properties Metric English Comments
Flexural Modulus 18.06 GPa
2619 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics LNP LUBRICOMP WCL36 PBT
LNP* LUBRICOMP* WCL36 is a compound based on PBT resin containing 30% Carbon Fiber, 15% PTFE. Added features of this grade include: Electrically Conductive, Wear Resistant.