Flexural Modulus 16.95 GPa
2458 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics LNP STAT-KON RE006 PA 66
LNP STAT-KON* RE006 is a compound based on Nylon 66 resin containing 30% Carbon Fiber. Added features of this material include: Electrically Conductive.