Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 1.655 GPa | 240.1 ksi | ASTM D790 |
Lucent Polymers CPP-110 Polypropylene Homopolymer, 10% Calcium Carbonate Filled Melt Flow Adjustable for ApplicationAdd "U" for UV StabilizedAdd "H" for Heat StabilizedInformation provided by Lucent Polymers, Inc. |