Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 15.91 GPa | 2308 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP UF00BAS PPA LNP* THERMOCOMP* UF00BAS is a compound based on Polyphthalamide containing 55% Glass Fiber. Added feature of this material is: Heat Stabilized. |
|||
Flexural Modulus | 15.91 GPa | 2308 ksi | ASTM D790 |
Saint-Gobain Meldin® 3140 Thermoplastic Bearing Material Meldin 3140 is an ideal thrust washer material and is well suited for thrust washer applications. Its high strength and stiffness, combined with its excellent heat dissipation properties, make it a.. |