Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 23.1 GPa | 3350 ksi | 1.3 mm/min; ASTM D790 |
PolyOne LubriOne™ SF2-30CF/15T Natural Polyphenylene Sulfide (PPS) LubriOne™ Lubricated and Wear-Resistant Compounds have been specifically formulated to be self-lubricating materials, offering low coefficient of friction and improved wear resistance properties. L.. |
|||
Flexural Modulus | 23.1 GPa | 3350 ksi | GB/T 9341-2008 |
Sichuan Deyang Haton® hCF41 Polyphenylene Sulfide Injection molding, high strengthInformation provided by Sichuan Deyang Chemical Co., LTD |