Polymer Property : Flexural Modulus = 2276 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 15.69 GPa
2276 ksi
ASTM D790
SABIC Innovative Plastics LNP THERMOCOMP PH1100B PA 6
LNP* THERMOCOMP* PH1100B is a compound based on Nylon 6 resin. Added feature of this material is: High Specific Gravity Filler. Added features of this material include: High Specific Gravity.