Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 1.517 GPa | 220.1 ksi | ASTM D790 |
Lucent Polymers TPP-320 Polypropylene, 20% Talc Filled, Impact Modified Melt Flow Adjustable for ApplicationAdd "U" for UV StabilizedAdd "H" for Heat StabilizedInformation provided by Lucent Polymers, Inc. |