Polymer Property : Flexural Modulus = 22.9 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 22.9 GPa
3320 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics LNP THERMOCOMP LC008EXP PEEK (Europe-Africa-Middle East)
LNP* THERMOCOMP* LC008EXP is a compound based on Polyetheretherketone containing Carbon Fiber. Added features include Electrically Conductive, Easy Molding.