Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | >= 1.49461 GPa | >= 216.775 ksi | ASTM D790 |
Buckeye Polymers BP RPP 2009 GK BLK Polypropylene, 20% Glass Filled Product Information: Our glass reinforced product lines exhibit increased tensile strength, stiffness, and heat deflection. Highly optimized glass reinforced PP resins have successfully replaced en.. |
|||
Flexural Modulus | >= 1.49461 GPa | >= 216.775 ksi | ASTM D790 |
Buckeye Polymers BP RPP 2012 TR BLK Polypropylene, Talc Filled Product Information: Our Talc filled product lines exhibit excellent properties such as high stiffness, surface aesthetics, low coefficient of thermal expansion, low shrinkage, improved scratch and .. |