Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 1.45 GPa | 211 ksi | ASTM D790 |
LyondellBasell Alathon® L5840 High Density Polyethylene ApplicationsALATHON L 5840 is a lightweight resin that exhibits excellent color, low odor and provides processing stability. Typical applications include household chemicals, industrial chemicals, .. |
|||
Flexural Modulus | 1.45 GPa | 211 ksi | 1% Secant, Injection Molded Sample, 0.05 in/min test speed; ASTM D790 |
Ineos N00N-00 Polypropylene Impact Copolymer Grade N00N-00 is a fractional melt flow rate, high impact copolymer polypropylene specifically designed for non-pressure structured wall pipe but can also be used in other extrusion applications req.. |