Polymer Property : Flexural Modulus = 21.2 GPa
Polymer Property :
Flexural Modulus =
21.2 GPa
Product List
Mechanical Properties
Tips:
30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties
Metric
English
Comments
Flexural Modulus
21.2
GPa
3070
ksi
GB/T 9341-2008
Sichuan Deyang Haton® hCF31 Polyphenylene Sulfide
Injection moldingInformation provided by Sichuan Deyang Chemical Co., LTD