Mechanical Properties Metric English Comments
Flexural Modulus 21.16 GPa
3069 ksi
ASTM D790
SABIC Innovative Plastics LNP THERMOCOMP OC006 PPS - Linear (Asia Pacific)
LNP* Thermocomp* OC006 is a compound based on PPS - Linear resin containing Carbon Fiber. Added features of this material include: Electrically Conductive.
Flexural Modulus 21.16 GPa
3069 ksi
ASTM D790
SABIC Innovative Plastics LNP STAT-KON OE006 PPS - Linear
LNP* STAT-KON* OE006 is a compound based on PPS - Linear resin containing 30% Carbon Fiber. Added features of this material include: Electrically Conductive.
Flexural Modulus 21.16 GPa
3069 ksi
ASTM D790
SABIC Innovative Plastics LNP THERMOCOMP OC006 PPS - Linear
LNP* THERMOCOMP* OC006 is a compound based on PPS-Linear resin containing 30% Carbon Fiber. Added features of this material include: Electrically Conductive.