Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 0.145 GPa | 21.0 ksi | ASTM D790 |
Ecomass® 4703BI62 Filled Polyurethane, Injection Molding Moderate Specific Gravity, Filled Polyurethane (TPU), Good Flexibility, Product Form - PelletsProcessing Method: Injection MoldingNontoxic alternative to Lead, radiation shielding applicationsInfor.. |
|||
Flexural Modulus | 0.145 GPa @Temperature 120 °C |
21.0 ksi @Temperature 248 °F |
ASTM Test |
BASF Ultramid® 8255 HS PA6 (Dry) Ultramid 8255 HS is a heat stabilized, impact modified type 6 nylon graft copolymer developed for both injection molding and extrusion applications. It exhibits varying levels of toughness and
fle.. |
|||
Flexural Modulus | 0.145 - 0.415 GPa @Temperature 65.0 - 120 °C |
21.0 - 60.2 ksi @Temperature 149 - 248 °F |
Average value: 0.262 GPa Grade Count:5 |
Overview of materials for Nylon 6, Impact Grade This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Impact Grade". Each property range of values reported is minimum and maximum values of appropri.. |