Mechanical Properties Metric English Comments
Flexural Modulus 13.96 GPa
2025 ksi
ISO 178
Polyplastics Duranex® CN7740XB Polybutylene Terephthalate (PBT), Super low warpage, GF filled
DURANEX® is a crystalline thermoplastic based on polybutylene terephthalate (PBT) that can be readily strengthened, modified, or otherwise performance enhanced through the addition of glass fibers ..