Polymer Property : Flexural Modulus = 200 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 200 - 230 GPa
29000 - 33400 ksi
Kennametal Stellite Denertiaâ„¢ C13 Cobalt Chromium Dental Alloy
Denertiaâ„¢ C13 is a cobalt chromium base-metal casting alloy for the manufacture of removable partial dentures and bridgework.This alloy is Nickel, Beryllium and Cadmium free as defined in ISO 6..
Flexural Modulus 200 - 230 GPa
29000 - 33400 ksi
Kennametal Stellite Denertiaâ„¢ C14 Cobalt Chromium Dental Alloy
Denertia™ C14 is a cobalt chromium base-metal casting alloy for the manufacture of removable partial dentures and bridgework. It conforms to the following International Standards: EN 1641 §..
Flexural Modulus 200 GPa
29000 ksi
Kennametal Stellite Denertiaâ„¢ N8 Nickel Dental Alloy
Denertiaâ„¢ N8 is a low-carbon nickel based porcelain-bonding alloy for the manufacture of dental crowns and bridges.This alloy is Beryllium and Cadmium free as defined by ISO 22674Information pr..
Flexural Modulus 200 - 230 GPa
29000 - 33400 ksi
Kennametal Stellite Denertiaâ„¢ C4 Cobalt Chromium Dental Alloy
Denertia™ C4 is a cobalt chromium base-metal casting alloy for the manufacture of removable partial dentures and bridgework.It conforms to the following International Standards: EN 1641 §4...