Polymer Property : Flexural Modulus = 20.92 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 20.92 GPa
3034 ksi
ISO 178
SABIC Innovative Plastics LNP THERMOCOMP 5C003 FP-V (PVDF)
LNP THERMOCOMP* 5C003 is a compound based on Polyvinylidene Fluoride resin containing 15% Carbon Fiber. Added features of this material include: Electrically Conductive.
Flexural Modulus 20.92 GPa
3034 ksi
ISO 178
SABIC Innovative Plastics LNP Thermocomp 5C003
LNP THERMOCOMP* 5C003 is a compound based on Polyvinylidene Fluoride resin containing Carbon Fiber. Added features of this material include: Electrically Conductive. Also known as THERMOCOMP* FP-VC..